It seems there is some difficulty in powder coating the pocket castings and feet from my Gold Crown 1. The castings keep out gassing causing small bubbling in the finish. Apparently, this is a common issue when powder coating cast material. I've considered plating and anodizing but both processes are quite expensive and anodizing cast material comes with its own challenges and pitfalls. If my powder coater is unable to achieve an acceptable finish, I am leaning toward the reproduction offerings below. Has anyone had any experience with these reproduction parts? Both are considerably more cost effective than replating my originals.
https://www.classicbilliards.net/an...s/chrome-finish-replacement-leg-levelers.html
https://www.ebay.com/itm/Billiard-P...rentrq:807c06b516e0a4b77cd14959ffefc5f0|iid:1
https://www.classicbilliards.net/an...s/chrome-finish-replacement-leg-levelers.html
https://www.ebay.com/itm/Billiard-P...rentrq:807c06b516e0a4b77cd14959ffefc5f0|iid:1
Last edited: