I think the west system 105 / 207 is the way to go if you want to use the epoxy. If have used G-5 and had 2 finished cues come up with a buzz from under the handle. I think the G-5 is too viscous and it leaves pockets during the install.
207 is a coating hardener.
206 is the slow hardener for bonding.
I think the west system 105 / 207 is the way to go if you want to use the epoxy. If have used G-5 and had 2 finished cues come up with a buzz from under the handle. I think the G-5 is too viscous and it leaves pockets during the install.
207 is a coating hardener.
206 is the slow hardener for bonding.